控制标准及物理性能指标
| 强度等级 | 抗压强度Mpa | 抗折强度Mpa | 水化热kj/kg | 干缩率% | 耐磨率 kg/m2 | 线膨胀率% | ||||||
| 3d | 7d | 28d | 3d | 7d | 28d | 3d | 7d | 28d | 28d | 7d | 28d | |
| 32.5 | ---- | 13.0~18.0 | 35.0~42.0 | ---- | 4.0~6.0 | 7.0~8.0 | 140~180 | 180~220 | 28天水化热≤280kj/kg | |||
| 42.5 | ---- | 15.0~20.0 | 48.0~52.0 | ---- | 4.5~6.5 | 7.5~9.0 | 180~220 | 200~250 | 28天水化热≤3000kj/kg; 90天抗压强度≥65Mpa | |||
| 代号强度等级 | 抗压强度Mpa | 抗折强度Mpa | 水化热kj/kg | 干缩率 | 耐磨率 | 线膨胀率 | |||||||
| 3d | 7d | 28d | 3d | 7d | 28d | 3d | 7d | 28d | 28d | 7d | 28d | ||
| P.O | 32.5 | ---- | ≥10.0 | ≥32.5 | ---- | ≥3.0 | ≥5.5 | ≤197 | ≤230 | ---- | ---- | ---- | ---- |
| 42.5 | ---- | ≥13.0 | ≥42.5 | ---- | ≥3.5 | ≥6.5 | ≤230 | ≤260 | ---- | ---- | ---- | ---- | |
内控标准
| 执行标准 | 内控标准 | 熟料 | |||||||||||
| LOSS% | MgO/% | SO3/% | R2O/% | f-CaO/% | Cl-/% | 不溶物/% | 比表面积 | 初凝min | 终凝min | C3S | C3A | C4AF | |
| GB/T 200-2017 | ≤2.0 | ≤3.0 | 2.3±0.2 | ≤0.5 | ≤1.0 | ≤0.03 | ≤0.55 | 320±10m²/kg | ≥90 | ≤300 | ≤50% | ≤5.0% | ---- |
低热硅酸盐水泥是以适当成分的硅酸盐水泥熟料加入适量石膏,经磨细制成的具有低水化热的水硬性胶凝材料。简称低热水泥,又称高贝利特水泥。